I need to travel down the road with a few pots to glaze in another kiln I can slow cool in. I am hoping to stiffen up the glazes so they don’t bump and fall off. They are cone 6 if I glaze and fire to say 08 will the glaze begin melt and be less likely to dust or flake off. I would try but kind of in a rush
Glaze travel
in Clay and Glaze Chemistry
Posted
I need to travel down the road with a few pots to glaze in another kiln I can slow cool in. I am hoping to stiffen up the glazes so they don’t bump and fall off. They are cone 6 if I glaze and fire to say 08 will the glaze begin melt and be less likely to dust or flake off. I would try but kind of in a rush