I have a dipping glaze for my classroom, but want to have a small bottle, do the students can brush it on as well. What should I add to the small bottle? Epsom Salts to keep it suspended? Gum solution so it dries slower?
- Show previous comments 5 more
-
REad Pete Pinnells article http://www.claytimes.com/articles/glazeadjusting.html Adjusting glazes
-
Takes a lot of CMC, so I make my own.
-
Thanks for the responses all. I went with a little bit of Epsom salt and gum solution. Initial test went well. Brushed on pretty evenly. I may have to tinker a bit more, but it's a start.