  1. Glaze firing on - mostly transparent over oxides and tissue transfers with my v reliable glossy glaze. On the shelf is a batch of stoneware pieces from a throwing workshop I attended - after 2 failed stoneware glaze firings I'm very reluctant to get on with these. Have tweaked the glaze and will do just one test piece before sacrificing the rest to the kiln gods

    1. Celia UK

      Celia UK

      Current firing is white earthenware - didn't make that clear! I too am no lover of glazing - after various disasters!

×
×