Hi I have a shelf or two that's empty in my glazefire, can I put some pieces in there that need to be bisque fired eventhough I'm firing that to cone 5? I usually bisque to cone 04. I just don't have any other glazed pieces right now and what's loaded is time sensitive, so I need to fire it this weekend. (student work)