  1. One of the art studios in town sells magic water, but I wasn't sure what it was. Do you have a recipe for it? Thanks -- I have several things to try now! The recepie is very simple, it will be much cheapper to make it yourself and one gallon will last! 3 tablespoons of sodium silicate, and 5 grams of soda ash to 1 gallon of water
  2. You should try Lana Wilson "Magic water" it did miracles for me in any stage of green ware, even on bone dry. Since I found the recepie, I don't work with out it. You will not have to wait for month for your pots to dry. :-) Happy creations!
×
×