Mark (Marko) Madrazo 187 Posted June 14, 2017 Report You made these? Are they 1/4" plexiglass? looks good. Quote Link to comment
Chilly 901 Posted June 14, 2017 Report My Dad and my partner between them. They are acrylic, some are 10mm and some are 6mm, and one is a mix of both. Quote Link to comment
Frankiegirl 3 Posted September 30, 2017 Report What are they connected with? I need these in my life Quote Link to comment
Chilly 901 Posted October 1, 2017 Report They are called U bolts. When we bought them, they came with two nuts each, had to buy extra nuts as you need four per bolt. Good luck, I love my hollow extruder dies. Quote Link to comment