ES10 Stoneware Cone 9 (electric)

Sign in to follow this  
From the album:

Jars, Mugs & Jugs

  • 12 images
  • 0 comments
  • 18 image comments

Photo Information for Experiment with glazes running and interacting

Taken with Canon Canon DIGITAL IXUS 70

  • 17.4 mm
  • 1/60
  • f f/4.9
  • ISO 80
View all photo EXIF information

Recommended Comments

And thankfully not too much movement ;-).  The main runs are from the yellowish Sandstone that is white when really thick. I use it as a base layer and also add a big dollop-ey third coat just below the rim. It applies in big drippy runs that freeze 1/4 of the way down and then run further when fired.

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.