9cm high. ES10 Stoneware Cone 9 (electric).

Quite pleased with the way the glazes turned out on this one, would appreciate your comments. Botz Tenmoku & Botz Satin Creme Matt

Sign in to follow this  
From the album:

Jars, Mugs & Jugs

  • 12 images
  • 0 comments
  • 18 image comments

Photo Information for 50ml Jug

Taken with Canon Canon DIGITAL IXUS 70

  • 14.4 mm
  • 1/60
  • f f/4.5
  • ISO 80
View all photo EXIF information

Recommended Comments

Glazes look lovely.
I think with the spout you have a couple things going on there, it could be a bit smaller as Nerd said but I also think it is angling down too much also. I would try pressing the side of your finger ever so slightly inwards and upwards just outside the lip at the same time as supporting the lip on the inside with another finger. Gives the spout a little lift and refines the shape of the spout. Do you think the body of the piece is wide enough to have a rim opening that size? Think I would play around with the proportions of the body versus the opening at the top. (if I knew how to add a picture here to explain the lip thing I would :wacko: )

Share this comment


Link to comment

Yes, something less flared at the top, perhaps just a small rolled rim.

 

Ummm, a rolled rim on a pitcher might turn into a dribbler. A sharp edge to cut the flow of liquid is a good idea. 

Share this comment


Link to comment

i think Min is referring to the style or lip that Robin Hopper shows in his several books.  

Is it there? I can't remember? It's something I've been doing with spouts for so long I don't really think about it. Kinda thought most potters do this?

Share this comment


Link to comment

OK so smaller spout and not flared. True it will need a sharp edge. I think I meant more like a simple thickening at the rim which would be easier to transition to an edge within the spout rather than a true roll.

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.