It is scary how thick the glaze must be to get this effect.

 

The oil spot 1 was sprayed on. Oil spot 2 was poured on - which was a first for me - never poured glaze onto a piece. Did 3 separate pours. Will cut it back to 2.

Link to comment

Yes. My test tile was dipped, 2 seconds for each glaze with SG 165-170, and it came out like this piece. Spraying has been a challenge. Each time the OS2 was sprayed too thin. Spray and wait till dry 3 times for the base, Oil spot 1. Then poured the Oil Spot 2.

 

This is very informative and worth trying Frank Vickery's way (there is a .pdf attachment about midways on this page) ---> http://cone6pots.ning.com/forum/topics/6-oil-spot-mfa-thesis

Link to comment

Just read your comments about thickness. Those iron black bases need to be super thick to get the above oilspot effect. I tried it with Pierre's Tenmoku and its absurd how thick that glaze has to be to look good. Otherwise. BROWN. 

 

Glad to see you got it going on. Looks great.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.