slip test



Using slip for texture and color disbursement. Spooned on and allowed to run off. After drying, a combination of a soft metal rib and sponge to rub off excess, and create textures. Slip had 0.25% cobalt carb added. Color is from nickel carb, magnesium carb, and Yellow Iron.

Copyright

© TJA 2016
From the album:

Crystalline Glaze / Tile

  • 16 images
  • 0 comments
  • 16 image comments

Photo Information for slip test

Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera

  • 5.7 mm
  • 100000/1000000
  • f f/2.9
  • ISO 160
View all photo EXIF information

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.