Turquoise stone and white matte ^6 ox on calico dark red clay. A couple very wonky vases that developed decent sized cracks from uneven drying, this was one of the first things I made after taking a hiatus of 3 years from clay, be gentle! I needed to keep a few unsatisfactory pieces to try my experiments. I am totally head over heals in love with the color combo, but am very sad all the pieces developed pin holes on them... I talked to the professor and she is going to go over how to avoid that next time and keep my work together as to have a more consistent firing.