oldlady

center tray is done at 5% copper carb, the others at 3 or 4. happier with the 5% but it has to be applied thickly.

From the album:

2016 fall pots

· 12 images
  • 12 images
  • 0 comments
  • 17 image comments

Photo Information

  • Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera
  • Focal Length 5.7 mm
  • Exposure Time 16667/1000000
  • f Aperture f/2.9
  • ISO Speed 80

Recommended Comments

Actually I prefer the 5% visually. The pin dot of deep green where the leaf would be attached to the stem is highlighted. To me that adds a great aesthetic, and follows what is commonly seen in nature.. My vote is for 5% 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.