Oxidation, glazed inside, raw clay on the outside.

From the album:

Glazed Ceramics 2013

  • 9 images
  • 0 comments
  • 8 image comments

Photo Information for Temmoku Red Clay Mortar and pestle

 Share


Recommended Comments

What clay is this and what cone is it fired to?? I like the form and style and color, a lot! Thanks! :)

 

Thank you! It is called Calico, it is a deep red clay that fires to this dark cherry color! It is sooo nice to work with, very soft yet holds its shape. This was fired to cone 6. 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.