Small test tile is formula T10 Coma Clay-crystal size 2.5". Bottom is cone 9 on regular Laguna porcelain- crystal size 1.75". Note also the clarity of the field color, and glaze checking is resolved.

Copyright

© TJA2016
From the album:

Clay Tests

  • 35 images
  • 0 comments
  • 34 image comments

Photo Information for ComaT10

Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera

  • 5.7 mm
  • 40000/1000000
  • f f/2.9
  • ISO 160
View all photo EXIF information
 Share


Recommended Comments

Are you satisfied with the T10 coma crystals? I think the crystal color looks more appealing in the Coma clay. It looks much more vibrant imo. The background looks more peach colored compared to the big tile which seems more brown, but it could just be angle of light.

 

Interesting stuff.

Link to comment

Joseph: yes I am in fact: usually I am not. Only thing I need to do is dial in the ramp hold temp to produce round floret crystals. T10 is a tank, the tile did not warp, which is common with standard porcelain. There is a distinct difference in field color as you noted: the standard cone 10 has much higher iron content. Going to throw some V-gum in and send you down a batch to play with. More than curious to see how your celadon works on it.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.