Saggarblueseaweedcurls copy



Re-fired a "non-remarkable" foil saggar piece with added seaweed and some copper

From the album:

July 2016 some favorite results

  • 19 images
  • 0 comments
  • 16 image comments

Photo Information for Saggarblueseaweedcurls copy

Taken with Panasonic DMC-FZ18

  • 4.6 mm
  • 1/100
  • f f/2.8
  • ISO 100
View all photo EXIF information

Recommended Comments

Yes-- this piece has a beautifully ethereal quality.

 

I am just beginning to appreciate that something good can come of re-firing, whether to rehabilitate a piece or just stretch things a bit.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.