first firing test kiln 014
results of firing slip tests at cone 6 oxidation. the white glaze on the right side is my standard Susan's white matte. it is from an apprentice of Charles Counts who taught me a lot of wonderful things about pottery. over a cobalt slip, the white disappears and leaves a smooth matte surface with the white only visible in the carved lines.