Jump to content

Rice Bowl 3


Marko
 Share


Cone 6, Precious White, Booter Blue, Green bean. My first bowls with my own glazes using a John Hesselberth base glaze.

From the album:

Bowls

  • 3 images
  • 0 comments
  • 12 image comments

Photo Information for Rice Bowl 3

Taken with samsung SM-G900P

  • 4.8 mm
  • 1/30
  • f f/2.2
  • ISO 320
View all photo EXIF information
 Share


Recommended Comments

nice stuff. fresh and animated. 

This is my first attempt at glaze making. I recommend John Hesselberth and Ron Roy's book; Mastering Cone 6 Glazes. They did all the hard work. I am glad I got it.

I have a few more glaze colors I want before I try other surface techniques, like Mattes, Satin or anything else.

Thanks for the kind words. I call it controlled chaos. It was fun.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.