Cone 6, Precious White, Booter Blue, Green bean. My first bowls with my own glazes using a John Hesselberth base glaze.

From the album:

Bowls

· 3 images
  • 3 images
  • 0 comments
  • 12 image comments

Photo Information

  • Taken with samsung SM-G900P
  • Focal Length 4.8 mm
  • Exposure Time 1/30
  • f Aperture f/2.2
  • ISO Speed 400

Recommended Comments

Very nice! is the blue cobalt?  

Yes, I used 1% Cobalt Carbonate and 3% Copper Carbonate. This is my first attempt at glaze making. So I was pleased that it worked out rather nice. 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.