Marcia Selsor 1,968 Posted April 13, 2016 Report Share I am still experimenting. Raised the shelf 1 inch, raised the size of the chamber by 1 brick, lowered the firing temperature and slowed the firing down a little. Same chemicals as always. Quote Link to comment