TJR 362 Posted February 8, 2016 Report Karen; I am liking your images-esp. the rabbit and the ravens.Great work! Tom [TJR] Quote Link to comment
karenkstudio 102 Posted February 9, 2016 Report Tom Thank you for the kind comments. karen Quote Link to comment
Mark (Marko) Madrazo 187 Posted February 11, 2016 Report You have a creative nature. Keep imagining more great artworks. Very nice. Try different wood backdrops. Maybe a cork or tree bark. Kudos. Quote Link to comment
AndreaB 56 Posted March 9, 2016 Report I really love this piece and would love it if you could share your method. No worries regarding me copying it though haha Quote Link to comment
karenkstudio 102 Posted March 9, 2016 Report Andrea All of the pieces for this tree were fired with a Raku glazes. that's how I get the metallic iridescent colors. The leaves and other pieces were arranged and glued to a pine board. Quote Link to comment