Upper parts of the hydria are starting to come together. The container is just over 18" tall at this stage and was wheel thrown in two parts, assembled on the wheel, allowed to dry for a few hours and then given the final shaping/neck-forming. With the addition of the footed-base, the greenware will stand just under 24" tall...that cannon happen until the base is hardened sufficiently to hold the weight of the upper portions.

Copyright

© Copyright 2016 - Paul Chenoweth - Nashville, TN - All rights reserved.
From the album:

Sketches by Paul

  • 11 images
  • 0 comments
  • 14 image comments

Photo Information for Hydria Work-in-Progress

Taken with Canon Canon PowerShot G16

  • 6.1 mm
  • 1/40
  • f f/1.8
  • ISO 400
View all photo EXIF information
 Share


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.