Carved poppy tumbler in Slate Blue, Side B
This one has the addition of iron oxide on just the flowers, stems and leaves, but I felt like it added very little so I won't bother next time. The glaze on its' own has a lovely break and brings out the design beautifully.
Copyright
© Copyright 2015 Giselle Massey, all rights reserved