Trinket dish with carved goldfish design. The carving was done after the piece was just past leather hard and heading to bone dry. I got a little chipping but with the design and glaze it looks pretty interesting. This is also a lesson in creating a spinner ... no footring and one of the clay supports slipped out of position when it was drying so it's a little wonky but it's on my desk!