Oh, man. This mug was such a beauty until I saw the dang spots where the glaze pickled on the inside and didn't fill in the bubble holes...hnngh. I didn't want to refire and risk the dragon's lines bleeding, and I couldn't BEAR to smash such a pretty mug, so I gave her to my fella. ^_^

Terracotta with white slip, ^03.

Copyright

© Sarah Alderete
From the album:

Early 2015

  • 12 images
  • 0 comments
  • 14 image comments

Photo Information for Dragon Rawr

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.