These are part of a commission for Distress Centre Calgary. They are given as corporate gifts, and read "Everyone is heard". I use a low tech silk screen (a plotter-cut Mylar sheet) to print the lettering onto a piece of newsprint, and gently apply this to the side of the mug. Once the slip is set up, I gently peel the newsprint off and apply the handles.

From the album:

Recent stuff

  • 8 images
  • 0 comments
  • 13 image comments

Photo Information for Fresh mugs with handles, even!

 Share


Recommended Comments

It's from a stencil that I push slip through. No screen to speak of, but I pull the slip over the stencil the same way you'd pull ink over an actual silk screen on to a piece of paper. Then the paper gets applied to a soft pot, because the stencil itself isn't flexible enough.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.