This bowl was a bit of a surprise. The interior is suposed to be chartreuse! Luckly the steel blue color is beautiful!

 

Black Mountain Clay with 3 coats of white Amaco Velvet Undeglaze, followed by 3 coats of chartreuse Amaco Velvet Underglaze before bisque firing. Then 3 coats of Amaco's zinc free clear fired to ^10. I also antiqued the outside with a cobalt oxide wash (which turns blue-black on the black mountain clay) to accent the texture.

 

The texture was carved into thick walls while the clay was leather hard.

Copyright

© Aug 2014

From the album:

Texture

· 2 images
  • 2 images
  • 0 comments
  • 1 image comment

Photo Information

  • Taken with Apple iPhone 5
  • Focal Length 4.1 mm
  • Exposure Time 1/143
  • f Aperture f/2.4
  • ISO Speed 50

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.