Brenda Turner 0 Posted September 14, 2020 Report Share I fired my first piece of glazed ceramics with the red brilliant gold to a cone 018. It did not shut off until after four hours and my piece was ruined. What did I do wrong ? I have orders for several of these pieces. Help. The cone looked as if it had barely bent ? Quote Link to comment
Brenda Turner 0 Posted September 14, 2020 Report Share The gold was old and I did shake it and thin a bit with essence but it still went on thick and tried to pool in spots. I tried to remove the pooling with a clean gold brush but I doubt this would have caused the stilts to melt all the way through the bottom on my piece? Quote Link to comment
Hulk 1,549 Posted September 15, 2020 Report Share Hi Brenda, Could you provide any details - what clay and glaze(s) did you use, what firing schedules (bisque and glaze), what are the problems ...and some pictures? Quote Link to comment
Recommended Comments