the pulp can be made in this contraption. Use hot water and add strips of paper or linter. beat until it looks like oatmeal.

From the album:

paper clay home made mixer

  • 3 images
  • 0 comments
  • 0 image comments

Photo Information for Mixerassembled smcopy

Taken with Panasonic DMC-FZ18

  • 4.6 mm
  • 1/13
  • f f/2.8
  • ISO 200
View all photo EXIF information
 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.