cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation   Whiting 18.5 Neph Syen 25.8 EPK 18.8 Silica 31.1 Gerstley B 4.6 98.8 Copper carb 0.3 Mason #6600 Black 0.02