I started recently and because I am interested in sculptural work this figure was an experiment

- I wanted to see how thick I can make a figure without it being hollow,

and without it cracking. (Thickest part was about an inch).

The legs sagged a bit because the figure had to lie flat while drying, but no cracks.

Any criticism/comments most welcome.

Photo Information for Figure, 12 inches high (30cm)

 Share


Recommended Comments

love the form, cant say i like the glaze though, that is just me, blue is one color that to me can look a bit hard. Have you considered to model this kind figure on a hangman style string. If you have not seen them you set up a piece of wood i use a right angle with a foot and clamp it to the work table. Then use a string as the plum line that goes through your figure. This keeps the legs totally straight and makes putting in a base super easy. Thanks for sharing your work, Trina

Link to comment

Thanks a lot Trina, I did not know about that, I will try it next time.

 

Bonnie-S 20 February 2012 - 11:00 PM

Have you tried paper clay? It is easy to make your own, or you can purchase it ready made. There is a DVD available for rent from SmartFlix or something like that. I have forgotten the name of the website. Or you can do a search for Paper Clay Videos in the Internet. It would be worth your while. The clay is fantastic for sculpture.

Link to comment

Its the same size that I have on my figurs. It is a good form but I am agree with trina. I my self use mangan or iron on leatherhard clay and wipe off the redundant. I throw a cone form and let it get leatherhard- then i form and build futher on. The head I form for itselves and let it get leatherhard before I glue it on. Excuse my English- hope you can understand what I mean! Keep up the good work wink.gif Best regards from Berte

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.