I recently participated in a wood firing at the red lodge Clay center #rlcc,
using the train kiln fired to ^12 and firing down in reduction for several hours to about 1900 F. I used several glazes and flashing slips as well as Helmar porcelain, Coleman porcelain, Babu porcelain and Death valley clay-a heavy iron bearing clay. I am very happy with the results.