I recently participated in a wood firing at the red lodge Clay center #rlcc,
using the train kiln fired to ^12 and firing down in reduction for several hours to about 1900 F. I used several glazes and flashing slips as well as Helmar porcelain, Coleman porcelain, Babu porcelain and Death valley clay-a heavy iron bearing clay. I am very happy with the results.

0 Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.