Sealer For Copper Raku?

15 May 2017 - 02:27 PM

what kind of a sealer can be used to slow oxidation of copper raku?
Beads I use for drop earrings have turned green.

Competive Juried Shows

21 July 2016 - 04:45 PM

Are there any benefits to entering competitive juried shows? I'm not referring to art and craft shows that offer booth space.
I have entered shows sponsored by organization in which I have a membership.

Wood Fired Bisque 06-04

29 June 2016 - 09:14 AM

Can anyone give me a tips on wood fired bisque ^06-04 with pieces to be glazed later.
I want to experiment using my wood-fired trash can raku kiln which can reach an ^08