Does anyone have a nice Cone 6 clear recipe?
Posted ImagePosted ImagePosted Image ... just kidding.

This is a Harry Memmott cone 6 clear glaze..good with underglazes and lustres and best of all...three ingredients!
Kaolin 15
Silica 35
Gerstley Borate 50
Let me know if you like it.