Posted by kathi on 19 August 2013 - 11:21 AM

Mel340 - You can get really cheap pads of newsprint from the art or craft store and it flexes a bit more than printer paper so is easier to wrap around a rounded form. You might try that and see if it helps you get a nice release.
I paid a little over a $100 for my printer which is pretty good I think. The toner cartridge lasts a long time too so even for printing other stuff it's cheaper to use than an inkjet.
I have Paul Wandless book as well plus a couple more all of which are super helpful in figuring this stuff out.

Terry

Even cheaper than pads of newsprint.....I go to the newspaper office and purchase the "end rolls."  These are the rolls of newsprint that only have one inch of paper left on them; not enough to leave on the press, but plenty to use....They charge me $1 apiece.




#29387 Bone Head Mistakes

Posted by kathi on 14 February 2013 - 03:03 PM

Have we all put a pot on the wheel to trim it, turned on the wheel without making sure pedal was off and had the pot (always a good one) fly across the room, or just me?