Tom Turners article on oxidized copper-reds is brilliant.
It does however emphasize the unavoidable truth that the only way to get the results you require is to spend time on testing and experimenting for yourself in your own conditions.
David Leach produced some beautiful `bullsblood` pots (early90`s), of which he was justifiably proud, but he never told me if they were reduced or not.