In Topic: Anyone Use Amaco Potters Choice Saturation Metallic Or Gold?

11 May 2013 - 06:24 AM

I tried the Paladium this weekend. Turned out a black-green with just a wee bit of metalic sheen. Ugly. I tried it on a small pinchpot and fired to ^6. My guess is it's overfired.

My friend whom I do pottery with uses the gold at cone 6, 04 bisque and it comes out true gold.