Topics I've Started

Gas Kiln Vs. Electric

19 December 2013 - 05:52 PM

I have always used an electric kiln, I'm a serious hobbiest. I am looking buy a new kiln and was considering a gas kiln. Any thoughts , advice would be appreciated.

Firing Plates

23 April 2013 - 04:30 PM

I have been making plates and other serving bowls and they are warping in the glaze kiln. I bisque fire at 06 and glaze at 6. I am using clay and glazes rated for that temp. Why are my pieces doing this? Thx!