Posted by dave the potter on 20 March 2014 - 02:34 PM

I agree, the cracks came in the cooling. Sometimes pots will crack if the have stuck to the shelf(glaze runs, glaze on the shelf, etc). The cooling shrinkage cannot happen correctly since the bottom of the pot will not move.