Shipping Lidded Vessels

20 November 2015 - 11:34 AM

Does anyone have any fabulous secret for shipping vessels with lids? I've had some breakage on the little handles on the top of the lid. I usually wrap it in bubble wrap and invert it in the vessel, but the holidays often have some rather heavy handed shippers.

 

I've been contemplating including a cardboard insert that keeps it from shifting side to side, which is most likely the key to the breakage.

 

Any input/help would be greatly appreciated.

Marc