Jump to content


SUS

Member Since 25 Sep 2010
Offline Last Active Oct 26 2010 01:23 PM
-----

Posts I've Made

In Topic: A Good ^6 Clear For Standard's 308 Brookland Red Clay

21 October 2010 - 09:47 AM

I sure willl ... may be a week or so. I will have to do a bisque first. Working in a Halloween party and camping trip into the mix of things too.

In Topic: Fired-On Images

19 October 2010 - 12:49 PM

Hey, I tried this a few years ago and got really good results, but then I tried to repeat using the same process, and the images burned away. I'm thinking that it may make a difference as to which glaze you have used, as some seem to eat the image.

In Topic: A Good ^6 Clear For Standard's 308 Brookland Red Clay

19 October 2010 - 12:11 PM

Many thanks to Tom and bciskpottery. Am trying to test with every new kiln fir. SUS

In Topic: Searching For Red Cone 6 Oxidation Glaze

27 September 2010 - 01:13 AM

Here is a site for iron red glazes to look over:

http://www.johnpost....pes-cone-6.html



I spent quite a long time looking at John Post's site last night. I found it very interesting and plan to test several of the glazes he generously offered. Also enjoyed seeing his studio and viewing his beautiful pots. Well worth viewing. SUS