In Topic: How to stop stamp sticking to clay

23 April 2013 - 02:31 PM

A light spray of WD-40 on your stamp will keep it from sticking and gives a good clean impression. You can usually make several impessions before having to spray again. I've used it to spray all sorts of things I've pressed into clay with excellent results. I've also used cornstarch but the impression isn't as crisp.

Marcia H.

In Topic: Ball milling glaze

13 March 2013 - 05:34 AM

What a profile picture, AtomicAxe. I wouldn't want to meet you in a dark alley.

Jim



Now that's the funniest thing I've read all morning. What a profiile picture, OffCenter. I wouldn't want to meet you in a dark alley either!