So I got busy and made three sinks for a house I am renovating. This past week I loaded them up and bisque fired them. One of the three survived the bisque firing. The good thing is I know how to efficiently make two more. Must allow more drying time for 1/2 inch thick ware this time..
Jan 05 2015 08:07 PM
  • Denice's Photo
    Denice
    I need to make a couple of sinks someday. The ones in my bath are chipping. Denice
    Jan 07 2015 09:04 AM
  • Marcia Selsor's Photo
    Marcia Selsor
    My friend made sinks and made a bowl to fire them in an upright position.
    Jan 08 2015 05:26 PM
  • JLowes's Photo
    JLowes
    I have new clay for the remake of two sinks, it's a nice architectural clay , very groggy. This time I will take more time to dry, and punch some relief holes inside the foot ring near the foot/bowl join to let the water out better.
    Jan 09 2015 11:53 AM
Photo

JLowes

I am getting loaded up for a show Saturday and Sunday in Norcross, Georgia. Just me, my honey, a hundred, or so, other artists and 50,000 people.
Oct 10 2014 12:36 PM
  • Min's Photo
    Min
    How did your sale go?
    Oct 13 2014 06:33 PM
Photo

JLowes

So I have half of my inventory I hope to take to my first show of Spring is in the kiln bisque firing. About two thirds are new designs I hope will sell well.
Apr 04 2014 08:54 AM
  • JLowes's Photo
    JLowes
    So, only one unsatisfactory pot in the whole load. A handle detached itself at the top join. It looks like someone forgot to score and slip...oops. Need to decide how to go...handle...no handle. All the raku destined pieces from the load are fired and turned out well.
    Apr 08 2014 09:16 AM
Photo

JLowesflorence w

Hello Florence W. THank you for your comment on my Avatar. It was inspired by my Yellow Labrador Retriever Lucy! She set me off on the raku animal quest, which is now my main direction for art/craft fairs and shows.
Jan 28 2013 03:50 PM
Photo

florence wJLowes

JLowes! I love your creation that you are using for your profile pix! Made me smile. Thanks! Florence W
Jan 28 2013 02:59 PM
Photo

WUVIEJLowes

I just adore your animal pottery!
Loved viewing your web page. :-)
Mar 04 2012 10:41 AM
Photo

JLowes

Potter Maintaining Training
Feb 06 2012 02:30 PM
Photo

Mark (Marko) MadrazoJLowes

I like your art. Especially the animal pots. I have your website in my favorites. I have not made a web site yet. Maybe someday when I have art as good as yours.
Nov 26 2011 04:52 PM