Do Glazes "spoil"?

16 April 2017 - 08:50 PM

My favorite white glaze has gone weird on me. It was made about 2 years ago and last used in September. I tried to use is night before last and noticed a change in the texture when I was stirring. It felt slimy. When I dipped a clean damp pot in it the glaze immediately started to flake off. I took it to the sink to wash the glaze off the pot. When water hit it the glaze it congealed (felt like sheet rock mud) and was hard to wash off the pot. Any thoughts?

 

White Silk c5-6

 

Dolomite 60 g

EPK 226 g

Flint 143g

GB 135g

Kona F4 300g

Neph Sy 592g

Talc 97.5g

Whiting 128g

Zinc Oxide 116g