In Topic: Ketchup Red Glaze

28 April 2015 - 12:39 PM

okay.. it has been so long since I have been here complaining about ketchup red not being red that I am not sure that this post will go out there somewhere BUT I need to tell someone that I just emptied my kiln with a whole load of ketchup red with glossy black over and black with ketchup red over. In my 20 years, I have never been so pleased with a glaze. Comes out almost black but with variation on raised areas. It doesn't leave my fnger prints, drips, messes, etc., just a beautiful shiney glaze. I just microwaved a piece and it didn't explode...  sometimes life is just good!