Josh Query's Bottle Form with "Manmade Shell Marks"

Posted By JBaymore on 27 April 2017 - 04:14 PM

Josh Query's Bottle Form with "Manmade Shell Marks"
This handbuilt bottle form shows the marks left by Josh Query's "manmade "seashells". The mix is 50% plaster, 50% whiting, and salt water to mix the stuff up with. Josh wanted shapes of marks that were more rectilinear than what naturally happens with scallop shells.

Was fired in the spring 2017 firing of New Hampshire Institute of Art's #Fushigigama. Was in the last rear stack of shelves.


Flower Vase

Posted By JBaymore on 23 April 2017 - 09:51 PM

Flower Vase
Wood fired flower vase with tenmoku glaze, applied feldspar, and red overglaze enamels.

This is sitting in the tokonoma (art alcove) in our newly renovated (2018-17) kitchen.


John Baymore Solo Exhibition 2017 -Thayer Gallery

Posted By JBaymore on 11 February 2017 - 08:31 PM

John Baymore Solo Exhibition 2017  -Thayer Gallery



John Baymore Solo Exhibition 2017 -Thayer Gallery

Posted By JBaymore on 11 February 2017 - 08:29 PM

John Baymore Solo Exhibition 2017  -Thayer Gallery



My Chawan used in Chakai at Urasenke Headquarters, Kyoto for Koicha

Posted By JBaymore on 13 October 2016 - 01:25 PM

My Chawan used in Chakai at Urasenke Headquarters, Kyoto for Koicha



40 Cubic Foot Gas Kiln Plan Example

Posted By JBaymore on 26 March 2016 - 08:22 PM

40 Cubic Foot Gas Kiln Plan Example
And example of one page of gas kiln plans.


Smokeless Anagama NHIA 2014

Posted By JBaymore on 20 February 2016 - 01:21 PM

Smokeless Anagama NHIA 2014
Anagama built in 2 weeks during the summer of 2014 by students in my kiln design and operation class at the New Hampshire Institute of Art. It fires completely smokeless and flameless at the top of the chimney.


Smokeless Anagama NHIA 2014

Posted By JBaymore on 20 February 2016 - 01:11 PM

Smokeless Anagama NHIA 2014
Anagama built in 2 weeks during the summer of 2014 by students in my kiln design and operation class at the New Hampshire Institute of Art. It fires completely smokeless and flameless at the top of the chimney.


Mugs

Posted By JBaymore on 11 July 2015 - 10:21 PM

Mugs
Two woodfired American style mugs. Local granite, local clay and wood ash glaze. Both were sold at a solo exhibition held in Japan in 2011.


Youhen Bottle Form

Posted By JBaymore on 10 September 2013 - 01:26 PM

Youhen Bottle Form
Thrown; yakishime; youhen charcoal finish; noborigama woodfired at Kanayamayaki, Goshogawara-shi, Aomori-ken, Japan; Orton cone 14. In my personal collection.


Youhen Flower Arranging Vase

Posted By JBaymore on 10 September 2013 - 01:22 PM

Youhen Flower Arranging Vase
Thrown; yakishime; youhen charcoal finish; noborigama woodfired at Kanayamayaki, Goshogawara-shi, Aomori-ken, Japan; Orton cone 14. Private collection in Japan.


Yakishime Gourd Shape Vase

Posted By JBaymore on 10 September 2013 - 01:16 PM

Yakishime Gourd Shape Vase
Thrown; yakishime; anagama woodfired at Tokyo National University of Fine Arts; Orton cone 13-14. In my personal collection.


American Shino Glaze Mizusashi (water jar for Japanese Tea Ceremony)

Posted By JBaymore on 10 September 2013 - 01:14 PM

American Shino Glaze Mizusashi (water jar for Japanese Tea Ceremony)
Thrown; noborigama woodfired; Orton cone 12; American Shino glaze. In the Tsinghua University collection in Beijing.