#107239 Newbie Needs Help With Glaze Cone 6 - Can It Really Be This Hard?

Posted by cstovin on 20 May 2016 - 09:05 PM

Thank you all; I didn't necessarily mean a three ingredient glaze would be "easy", but easier in terms of only three ingredients to potentially trouble shoot, and much less to spend at first :)

 

I liked the comment about cheating lol

 

Thank you for suggesting it go on heavier, I thought the second time around two coats would be good; and I did mix it with a little less water but will try it again 

C.




#33121 One more on glass infused pottery

Posted by cstovin on 17 April 2013 - 03:51 PM

Thank you, PomPots, I will get my questions together and post them.....most of the items I do now are decorative, so crazing isn't too much of a concern for me now; but I just wanted to get more information and can't find much! Will try the search terms you suggested also -