Firing schedule

13 June 2013 - 12:46 PM

I am not sure how to program my kiln to do this kind of schedule for a crystal glaze...can anyone who knows explain it? Also can I firinf other pieces in this firing or only the crystal glazes?


Segment

Rate

Temp.

Hold

1

250°/hour

1250°F

0

2

350°/hour

2140°F

0

3

25°/hour

2165°F

0

4

9999 setting

1950°F

3 hrs.



Would appreciate any help with this confusing glaze firing schedule.

need recipe for making molds

17 August 2012 - 10:44 AM

Good morniing!

I am in need of a way to make molds by mixing some material, such as white cement and gesso...I am not sure if anything else is needed or if I am using the right terms.
I live in South America and things are not labeled the same.

If anyone knows a recipe for making these plaster "type" molds for ceramic tiles, I would really appreciate your help.