In Topic: Looking For Grey Cone 6 Ox Recipe

11 November 2013 - 05:27 PM

Okay, I have 2 good gray recipes at my studio, next time im by there ill write down the recipes and post them.

In Topic: Oxide Wash

07 November 2013 - 08:27 PM



My favorite oxide wash is a Rutile wash, just mix 50% rutile, 48% gerstley borate, and 2% bentonite. Mix with water until about skim milk consistency. This provides a warm yellow on majolica, a great brown at midfire, and a really cool textured orange under celadon at ^11.




P.s. Bienvenue! Je suis content que vous utilisez cette grande ressource pour vos questions et préoccupations!

In Topic: Glaze Help Needed!

07 November 2013 - 08:06 PM

You could also try adding CMC gum solution, a commercial suspension agent, or glycerin a tablespoon at a time.



In Topic: Looking For Grey Cone 6 Ox Recipe

07 November 2013 - 08:01 PM

I have a few recipes, if you want them, however adding a black stain to a white matte is the easiest solution.



In Topic: "Stuff"

16 June 2013 - 11:29 PM

Im collecting cow dung ash and dirt from various places. I figure that I can make an ash glaze and a slip.