#87726 Qotw: • What Is The Best Advice Anyone Has Ever Given You?

Posted by 123pop on 24 June 2015 - 02:45 PM

"Don't be afraid to be afraid".  Not sure who said it but words  to push you to new heights.

 

About liking pots later....some pots came out of the kiln not what I expected so I immediately gave them to a friend (she liked them).  A year later or so I was at her house. I saw these lovely pots and asked where she got them.  She said from you.  I loved them...the glaze was quite nice and colorful.  You just never know.




#65368 How Best To Dry Reclaimed Dried Clay After It Has Been Processed Into Wet Clay

Posted by 123pop on 30 August 2014 - 05:28 AM